◆GH2132 (incoloyA-286/S66286) yana da kyakkyawan aiki gaba ɗaya da iyakar yawan amfanin ƙasa. Ana amfani da shi don fayafai na injin turbine, jikin zobe, welding bracket da kayan sassan diyya ƙasa da 700 ° C.
◆GH3030 gami yana da tsayayyen tsari, ƙarancin tsufa, da juriya mai kyau na iskar shaka. Ya dace da ɗakunan konewa da masu ƙonewa a ƙasa da 800 ° C.
◆GH3128 yana da kyau m yi, high karko, mai kyau hadawan abu da iskar shaka juriya, mai kyau tsarin kwanciyar hankali da kuma mai kyau waldi aiki, da aka yafi amfani ga konewa jam'iyya da afterburner sassa na turbine engine tare da wani aiki zafin jiki na 950 ° C.
◆GH4145 (inconelx-750/N07750) yana da isasshen ƙarfi, lalata juriya da hadawan abu da iskar shaka juriya a kasa 980 ° C. Abu ne da aka fi so don maɓuɓɓugan ruwa mai ƙarfi kuma ya dace da yin diaphragms na roba da zanen gado na roba.
GH4169 (N07718 / inconel718) yana da tsarin austenite, kuma lokacin "Y" wanda aka kafa bayan hazo yana sa ya sami kyawawan kayan aikin injiniya. Ana amfani dashi sosai a wurare daban-daban tare da buƙatun juriya na zafin jiki.
GH4080A (N07080/Nimonic80A)Z yana da isasshen zafin jiki mai zafi a 700-750°C da kyakkyawan juriyar iskar oxygen ƙasa 900°C. Wannan gami na musamman ya dace da filayen da ke buƙatar ƙarfin ƙarfi da juriya na lalata.
◆GH3044 Babban ɗakin konewa da abubuwan da suka shafi bayan gida, garkuwar zafi, vanes na jagora, da sauransu.
GH4080A yana da kyau mai rarrafe juriya da hadawan abu da iskar shaka juriya a cikin kewayon 650-850 ° C.
◆GH2136 yana da kyau overall yi, barga tsarin bayan dogon lokaci amfani, mai kyau hadawan abu da iskar shaka juriya, kananan mikakke fadada coefficient, da kuma sauki waldi da kafa.
◆GH2036 Fayafai na Turbine, garkuwar zafi, zoben riƙewa, zobba masu ɗaukar nauyi, ɗakuna, da sauransu waɗanda ke aiki ƙasa da 650 ° C.
◆GH4738 ya dace don yin fayafai na injin turbine, ruwan wukake masu aiki, masu zafi masu zafi, bututun wuta, shafts da turbines, da sauransu.
Abubuwan sinadaran
Daraja | C | Si | Mn | S | P | Cr | Co | W | Mo | Ti | Al | Fe | Ni | sauran |
babu girma fiye | ||||||||||||||
GH2132 | 0.08 | 1 | 2 | 0.02 | 0.03 | 13.5 zuwa 16 | - | - | 1 zuwa 1.5 | 1.75 zuwa 2.35 | ≤0.4 | tushe | 24 zuwa 27 | B: 0.001 ~ 0.01 V: 0.1 ~ 0.5 |
GH3030 | 0.12 | 0.8 | 0.7 | 0.02 | 0.03 | 19 zuwa 22 | - | - | - | 0.15 zuwa 0.35 | ≤0.15 | ≤1.5 | tushe | - |
GH3128 | 0.05 | 0.8 | 0.5 | 0.013 | 0.013 | 19 zuwa 22 | - | 7.5 zuwa 9 | 7.5 zuwa 9 | 0.4 zuwa 0.8 | 0.4 zuwa 0.8 | ≤2.0 | tushe | B≤0.005 Ce≤0.05 Zr≤0.06 |
GH4145 | 0.08 | 0.5 | 1 | 0.01 | 0.015 | 14 zuwa 17 | ≤1 | - | - | 2.25 zuwa 2.75 | 0.4 zuwa 1 | 5 zuwa 9 | ≥70 | Nb: 0.7 ~ 1.2 |
GH4169 | 0.08 | 0.35 | 0.35 | 0.015 | 0.015 | 17 zuwa 21 | ≤1 | - | 2.8 zuwa 3.3 | 0.65 ~ 1.15 | 0.2 zuwa 0.8 | Ci gaba | 50 ~ 55 | Ku ≤0.3 Nb4.75 ~ 5.5 Mg≤0.1 B≤0.006 |
GH4080A | 0.04 zuwa 0.1 | 1 | 1 | 0.015 | 0.02 | 18 zuwa 21 | ≤2 | - | - | 1.8 zuwa 2.7 | 1.1.8 | - | ≥65 | Ku≤2 B≤0.006 |
GH3044 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 zuwa 26.5 | - | 13 zuwa 16 | ≤1.5 | 0.3 zuwa 0.7 | ≤0.5 | ≤4.0 | tushe | Ku ≤0.07 |
GH2136 | 0.06 | 0.75 | 0.35 | 0.025 | 0.025 | 13 zuwa 16 | - | - | 1.75 | 2.4 zuwa 3.2 | ≤0.35 | tushe | 24.5 zuwa 28.5 | B: 0.005 ~ 0.025 V: 0.01 ~ 0.1 |
GH2036 | 0.34 zuwa 0.4 | 0.3 zuwa 0.8 | 7.5 zuwa 9.5 | 0.03 | 0.035 | 11.5 zuwa 13.5 | - | - | 1.1-1.4 | ≤0.12 | - | tushe | 7 zuwa 9 | V: 1.25 ~ 1.55 Nb: 0.25 ~ 0.5 |
GH4738 | 0.03 zuwa 0.1 | 0.15 | 0.1 | 0.015 | 0.015 | 18 zuwa 21 | 12 zuwa 15 | - | 3.5 zuwa 5 | 2.75 zuwa 3.25 | 1.2-1.6 | ≤2.0 | tushe | B: 0.003 ~ 0.01 Zr: 0.02 ~ 0.08 |
Alloy dukiya m
jihar | Ƙarfin ƙarfi RmN/m㎡ | Ƙarfin Haɓaka Rp0.2N/m㎡ | Tsawaita Kamar% | Brinell hardness HB |
Magani Magani | 610 | 270 | 30 | ≤321 |
Magani Magani | 650 | 320 | 30 | - |
Magani Magani | 735 | 340 | 40 | - |
Magani Magani | 910 | 550 | 25 | ≤350 |
Magani Magani | 965 | 550 | 30 | ≤363 |
Magani Magani | 845 | 340 | 48.5 | - |
Magani Magani | 920 | 550 | 25 | - |
Magani Magani | 950 | 700 | 20 | - |
Magani Magani | 850 | 600 | 15 | - |
Magani Magani | 1111 | 741 | 21.5 | 24.5 |