Incoloy
Haɗaɗɗen Zazzabi
◆Incoloy800H (Ns112 / N08810), Incoloy800HT, Incoloy800 (Ns111 / N08800) ne uku kayayyakin na wannan nickel-baƙin ƙarfe-chromium gami jerin, suna da kyau lalata juriya, creep juriya da kuma high zafin jiki juriya, ana amfani da hadaddun hadawan abu da iskar shaka juriya. jiyya Kayan aikin shigarwa, na'urorin rufewa don juriya ga jikin tubular dumama, sinadarai da kayan sarrafa man fetur.
◆Incoloy825 (Ns142/N08825) kayan aikin injiniya ne na gabaɗaya. Yana da anti-acid da alkali karfe lalata juriya a duka oxidizing da rage muhalli. Babban abun ciki na nickel yana sa gami ya sami juriyar lalatawar damuwa. Ana amfani da shi sosai a fannonin masana'antu daban-daban inda zafin aiki bai wuce 550 ° C ba.
◆Incoloy901 shine hazo hardening, creep zafi resistant karfe. Alloy yana da ƙarfin yawan amfanin ƙasa da ƙarfi mai ɗorewa a ƙasa 650 ° C, kyakkyawan juriya na iskar shaka a ƙasa 760 ° C, kuma yana da kwanciyar hankali don amfani na dogon lokaci. An yi amfani da shi sosai wajen kera sassa kamar sassa masu juyawa na jirgin sama da injin turbin gas da ke aiki ƙasa da 650 ° C.
◆Incoloy925 (N09925) wani gami karfe ne mai kyau inji ƙarfi da kuma m lalata juriya. Ana yawan amfani da shi wajen kera sassa akan hakar mai da iskar #kayan.
◆Incoloy926 wani bakin karfe ne na austenitic mai irin wannan sinadari mai kama da alloy 904L, abun cikinsa na nitrogen ya karu zuwa kusan 0.2%, kuma abun cikin molybdenum shine 6.5%. Yafi amfani da marine injiniya, acid gas yanayi, flue gas desulfurization tsarin.
◆Incoloy20 wani nau'i ne na kayan ƙarfe wanda zai iya aiki na dogon lokaci a ƙarƙashin yanayin zafi da ke ƙasa da 600 ℃ da wasu damuwa.
◆Incoloy330 yana da babban ƙarfi, mai kyau oxidation juriya, lalata juriya, mai kyau gajiya juriya, karaya taurin da sauran kaddarorin, kuma ya dace da makamashin nukiliya, sinadaran masana'antu, da sauran inji filayen.
Abubuwan sinadaran
Daraja | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | sauran |
babu girma fiye | |||||||||||||
Incoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 zuwa 23 | 30 zuwa 35 | tushe | 0.15 zuwa 0.6 | 0.15 zuwa 0.6 | ≤0.75 | - | - |
Incoloy800H | 0.05 zuwa 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 zuwa 23 | 30 zuwa 35 | tushe | 0.15 zuwa 0.6 | 0.15 zuwa 0.6 | ≤0.75 | - | - |
Farashin 800HT | 0.06 zuwa 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19 zuwa 23 | 30 zuwa 35 | tushe | 0.15 zuwa 0.6 | 0.15 zuwa 0.6 | ≤0.75 | - | Al+Ti 0.85 ~ 1.2 |
Farashin 825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5 zuwa 23.5 | 38 zuwa 46 | tushe | ≤0.2 | 0.6 zuwa 1.2 | 1.5 zuwa 3 | 2.5 zuwa 3.5 | - |
Farashin 901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11 zuwa 14 | 40 zuwa 45 | tushe | ≤0.35 | 2.35 zuwa 3.1 | ≤0.5 | 5 zuwa 7 | Co≤1.0 |
Farashin 925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5 zuwa 23.5 | 42 zuwa 46 | tushe | 0.15 zuwa 0.5 | 1.9 zuwa 2.4 | 1.5 zuwa 3 | 2.5 zuwa 3.5 | - |
Farashin 926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19 zuwa 21 | 24 zuwa 26 | tushe | - | - | 0.5 zuwa 1.5 | 6 zuwa 7 | N15~0.25 |
Farashin 020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 zuwa 26.5 | - | 13 zuwa 16 | ≤1.5 | 0.3 zuwa 0.7 | ≤0.5 | 2.5 zuwa 3.7 | - |
Farashin 330 | 0.04 zuwa 0.08 | 1 zuwa 1.5 | 2 | 0.03 | 0.03 | 18 zuwa 20 | 34 zuwa 37 | tushe | - | - | ≤1 | - | - |
Alloy dukiya m
Daraja | jihar | Ƙarfin ƙarfi RmN/m㎡ | Ƙarfin Haɓaka Rp0.2N/m㎡ | Tsawaita Kamar% | Brinell hardness HB |
Incoloy800 | Magani Magani | 500 | 210 | 35 | - |
Incoloy800H | Magani Magani | 450 | 180 | 35 | - |
Farashin 800HT | Magani Magani | 500 | 210 | 35 | - |
Farashin 825 | Magani Magani | 500 | 220 | 30 | - |
Farashin 901 | Magani Magani | 900 | 550 | 25 | - |
Farashin 925 | Magani Magani | 650 | 300 | 30 | - |
Farashin 926 | Magani Magani | 650 | 295 | 35 | - |
Incoloy20 | Magani Magani | 700 | 300 | 32 | - |
Farashin 330 | Magani Magani | 750 | 310 | 35 | - |