Monel
Haɗaɗɗen Zazzabi
◆Monel400 yana da kyakkyawan juriya na lalatawa a cikin hydrofluoric acid da iskar fluorine, kuma ya dace da kayan aikin bututu da bawuloli da ake amfani da su a masana'antar sinadarai, man fetur, makamashin atomic, da haɓakar ruwa.
◆Monel500 yana da kyau m inji Properties, high ƙarfi da kyau lalata juriya. Ya dace da masu ɗaure da sassa na tsarin da ake amfani da su a masana'antar sinadarai, jiragen ruwa da injiniyan ruwa.
◆Monel404 ne yadu amfani a petrochemical, nukiliya masana'antu, da sauran yankan-baki masana'antu sassa.
Abubuwan sinadaran
Daraja | C | Si | Mn | S | P | Cr | Ni | Mo | Fe | Co | W | Al | Ti | Cu |
babu girma fiye | ||||||||||||||
Monel400 | 0.3 | 0.5 | 2 | 0.024 | - | - | tushe | - | ≤2.5 | - | - | - | - | 28 zuwa 34 |
Kudin 500 | 0.18 | 0.5 | 1.5 | 0.01 | - | - | ≥63 | - | ≤2 | - | - | 2.3 zuwa 3.15 | 0.35 zuwa 0.85 | 27 zuwa 33 |
Kudin404 | 0.15 | 0.1 | 0.1 | 0.024 | - | - | 52 zuwa 57 | - | ≤0.5 | - | - | ≤0.05 | - | Ci gaba |
Alloy dukiya m
Daraja | Yanayin fasaha | Ƙarfin ƙarfi RmN/m㎡ | Ƙarfin Haɓaka Rp0.2N/m㎡ | Tsawaita Kamar% | Brinell hardness HB |
Monel400 | Ƙirƙira / zafi birgima | 516 | 170 | 35 | - |
Jihar da aka soke | 483 | 170 | 35 | - | |
Kudin 500 | Juyin yanayi + tsufa | 960 | 686 | 20 | 27 |
m bayani + tsufa | 896 | 585 | 20 | 24 | |
Kudin404 | Jihar da aka soke | 550 | 185 | 36 | - |