Nitronic
Haɗaɗɗen Zazzabi
◆Nitronic50 (S20910/XM-19) wani bakin karfe ne da aka inganta shi da sinadarin nitrogen, wanda aka fi amfani dashi a masana'antar petrochemical, yadi, sarrafa abinci da masana'antar ruwa.
◆Nitronic60 (S21800 / Alloy218) yana da kyau kwarai high-zazzabi hadawan abu da iskar shaka juriya da kuma low-zazzabi tasiri yi, da aka yafi amfani da tasiri anti-sawa da karce gami gada fil da sauran key ayyukan.
Abubuwan sinadaran
Daraja | C | Si | Mn | S | P | Cr | Ni | Fe | Mo | Ti | Cu | Nb | N | sauran |
babu girma fiye | ||||||||||||||
Nitronic50 | 0.06 | 1 | 4 zuwa 6 | 0.03 | 0.04 | 20.5 zuwa 23.5 | 11.5 zuwa 13.5 | tushe | 1.5 zuwa 3 | - | - | 0.1 zuwa 0.3 | 0.2 zuwa 0.4 | - |
Nitronic 60 | 0.1 | 3.5 zuwa 4.5 | 7 zuwa 9 | 0.03 | 0.04 | 16 zuwa 18 | 8 zuwa 9 | tushe | - | - | - | - | 0.08 zuwa 0.18 | - |
Alloy dukiya m
Daraja | jihar | Ƙarfin ƙarfi RmN/m㎡ | Ƙarfin Haɓaka Rp0.2N/m㎡ | Tsawaita Kamar% | Brinell hardness HB |
Nitronic50 | Magani Magani | 690 | 380 | 35 | - |
Nitronic 60 | Magani Magani | 600 | 320 | 35 | - |