Monel
Haɗaɗɗen Haɗaɗɗen Haɗaɗɗen Zazzabi Grade C Si Mn SP Cr Ni Mo Fe Co W Al Ti Cu bai fi Monel400 0.3 0.5 2 0.024 - - tushe - ≤2.5 - - - - 28~34 Monel500 0.18 0.5 1.5 0.06 - ≤2 - 2.3 ~ 3.15 0.35 ~ 0.85 ~ 0.85 ~ 33 75 0.1.05 - - - - - - - --- ci gaba da zama mallakin kayan aikin fasaha ... -
Austenite Bakin Karfe
Haɗaɗɗen Haɗaɗɗen Haɗaɗɗen Zazzabi Grade C Si Mn SP Cr Ni Mo Cu N wani bai wuce 904L 0.02 1 2 0.015 0.03 19~21 24~26 4~5 1~2 - - 253Ma 0.05~ ~22 10~12 - - 0.14~0.2 Ce0.03~0.08 254SMo 0.02 0.8 1 0.01 0.03 19.5~20.5 17.5~18.5 6~0.6.5 N 0.03 1 2 0.03 0.04 20-22 23.5~ 25.5 6~7 ≤0.75 0.18~... -
Siffar, Flat, Square, Zagaye, Fine, Plated and Bare Waya ASTM A167, AMS 5523
Alloy 310S ne austenitic chromium nickel bakin karfe wanda ke da kyakkyawan juriya na iskar shaka da ƙarfi a yanayin zafi mai tsayi a ci gaba da sabis har zuwa 2000ºF (idan an ba da rage gasses sulfur ba a nan).Hakanan ana amfani dashi don sabis na wucin gadi a yanayin zafi har zuwa 1900F saboda yana ƙin sake gyarawa kuma yana da ƙarancin haɓakar haɓakawa.Wannan al'amari yana rage halayen karfe don yin zafi a sabis na zafi.Alloy 310S yayi kama da alloy 310 ban da ƙananan abun ciki na carbon don rage hazo carbide yayin walda.
-
Hazo Hardening Bakin Karfe
High Temperate Alloy Chemical Complex Grade C Si Mn SP Cr Ni Mo Cu Nb Al sauran wanda bai fi 0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5~17.5 3~5 - 3~5 0.15~1 -0.0C .035 0.03 16 zuwa 18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - - 0.75 - 0Cu 0.035 0.03 14 zuwa 15.5 3.5 ... -
ALLOY 625 BAYANIN BAYANIN DATA
Alloy 625 wani nonmagnetic ne, lalata - kuma mai jurewa iskar shaka, gami da tushen nickel.Ƙarfinsa na ban mamaki da taurinsa a cikin kewayon zafin jiki na cryogenic zuwa 2000 ° F (1093 ° C) an samo shi ne da farko daga ingantaccen tasirin maganin ƙarfe na refractory, columbium da molybdenum, a cikin matrix nickel-chromium.Garin yana da kyakkyawan ƙarfin gajiya da damuwa-lalata juriya ga ions chloride.Wasu aikace-aikace na al'ada don gami 625 sun haɗa da garkuwar zafi, kayan aikin makera, injin injin turbin gas, layin konewa da sandunan feshi, kayan aikin shuka sinadarai, da aikace-aikacen ruwan teku na musamman.
-
Bakin Karfe 904L 1.4539
Wannan takardar bayanan ta shafi bakin karfe 904L / 1.4539 zafi da sanyi birgima takardar da tsiri, samfuran da aka kammala, sanduna, waya mai birgima da bayanan martaba da kuma bututun da ba su da kyau da walda don dalilai na matsa lamba.
-
Inconel
Haɗaɗɗen Haɗaɗɗen Haɗaɗɗen Zazzabi Grade C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb wanin wanda bai fi Inconel600 0.15 0.5 1 0.015 0.03 14~17 tushe 6~10 - - ≤0.5 - - - Inconel601 0.03 25 tushe 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 tushe ≤5 ≤0.4 ≤0.4 - 8~150≤0.5 0.2 0.35 0... -
Hastelloy C-276 BAYANIN DATA
HASTELLOY C276, UNS N10276 ana ɗaukarsa mafi yawan juriyar lalata nickel gami da ake samu.Har ila yau, Alloy C-276 yana da kyakkyawan juriya ga pitting, damuwa-lalacewa, musamman dacewa don amfani a cikin matsanancin zafin jiki, inorganic acid da Organic acid gauraye da ƙazanta (irin su formic acid da acetic acid), da kuma wuraren lalata ruwa na teku.
-
Alloy
Haɗaɗɗen Haɗaɗɗen Haɗaɗɗen Zazzabi Grade C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb wanin wanda bai fi Inconel600 0.15 0.5 1 0.015 0.03 14~17 tushe 6~10 - - ≤0.5 - - - Inconel601 0.03 25 tushe 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 tushe ≤5 ≤0.4 ≤0.4 - 8~150≤0.5 0.2 0.35 0... -
ALLOY 600 MATERIAL DATA SHETES
Farashin INCONEL 600
Inconel Alloy 600 A nickel-chromium alloy tare da kyakkyawan juriya na iskar shaka a yanayin zafi da juriya ga chloride-ion stress-corrosion cracking, lalata ta ruwa mai tsabta, da lalata caustic.An yi amfani da shi don abubuwan da aka gyara na tanderu, a cikin sinadarai da sarrafa abinci, a aikin injiniyan nukiliya, da kuma na wutar lantarki.
Saukewa: N06600
Saukewa: 2.4816
-
HASTELLOY B2 UNS N10665 W.NR.2.4617
Hastelloy B2 shine ingantaccen bayani wanda aka ƙarfafa, gami da nickel-molybdenum, tare da juriya mai mahimmanci don rage yanayi kamar iskar hydrogen chloride, da sulfuric, acetic da phosphoric acid.Molybdenum shine kashi na farko na alloying wanda ke ba da juriya mai mahimmanci don rage yanayin.Wannan nickel karfe gami za a iya amfani da a matsayin-welded yanayin domin shi tsayayya da samuwar hatsi-iyaka carbide precipitates a cikin weld zafi-shafi yankin.
Wannan nickel gami yana ba da kyakkyawan juriya ga hydrochloric acid a kowane taro da yanayin zafi.Bugu da ƙari, Hastelloy B2 yana da kyakkyawan juriya ga rami, damuwa da lalata da kuma zuwa layin wuka da harin yankin da zafi ya shafa.Alloy B2 yana ba da juriya ga tsantsar sulfuric acid da adadin acid marasa ƙarfi.
-
Hastelloy
Babban Zazzabi Alloy Chemical abun da ke ciki Grade CPS Mn Si Ni Cr Co Cu Fe N Mo Al WV Ti wani mafi girma fiye da HastelloyB 0.05 0.04 0.03 1 1 tushe ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - -B -2 0.02 0.04 0.03 1 0.1 tushe ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB 3 0.01 0.04 0.03 3 0.1 ≥65 1~3 32 ≤0.5 ≤ 3 ≤0.2 ≤0.2 - ...