◆Alloy20cb-3 yana da kyau kwarai juriya ga danniya lalata fatattaka da kyau juriya ga gida rage fili fili lalata lalata, kuma ana amfani da sulfuric acid yanayi da kuma masana'antu shigarwa na sulfuric acid bayani dauke da halogen ions da karfe ions.
◆Alloy28 ana amfani dashi sosai wajen yin takarda, magunguna, sinadarai, kare muhalli, ginin jirgi da sauran masana'antu.
◆Alloy31 (N08031/1.4562) wani sinadarin nitrogen ne mai dauke da iron-nickel-molybdenum gami wanda aikinsa ya kasance tsakanin super austenitic bakin karfe da kuma hadaddiyar giyar da ke da nickel.Ya dace da sinadaran da petrochemical, injiniyan muhalli da samar da mai da iskar gas, da dai sauransu filin masana'antu.
◆Alloy33 wani nau'i ne na kayan ƙarfe wanda ke aiki na dogon lokaci a ƙarƙashin babban zafin jiki na 600-1200 ℃ da wasu damuwa.Yana da high high high zafin jiki ƙarfi, mai kyau anti-oxidation da anti-lalata yi.
◆Alloy75 yana da kyau nama kwanciyar hankali da sabis AMINCI a karkashin high zafin jiki yanayi, kuma ya dace da sararin samaniya, jirgin sama, man fetur, sinadaran masana'antu, da kuma wani muhimmin abu ga jiragen ruwa.
Abubuwan sinadaran
Daraja | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | sauran |
babu girma fiye | ||||||||||||||
Inconel600 | 0.15 | 0.5 | 1 | 0.015 | 0.03 | 14 zuwa 17 | tushe | 6 zuwa 10 | - | - | ≤0.5 | - | - | - |
Farashin 601 | 0.1 | 0.5 | 1 | 0.015 | 0.03 | 21 zuwa 25 | tushe | 10 zuwa 15 | 1.1.7 | - | ≤1 | - | - | - |
Farashin 625 | 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20 zuwa 23 | tushe | ≤5 | ≤0.4 | ≤0.4 | - | 8 zuwa 10 | 3.15 zuwa 4.15 | Co≤1 |
Inconel725 | 0.03 | 0.2 | 0.35 | 0.01 | 0.015 | 19 zuwa 22.5 | 55 zuwa 59 | Ci gaba | 0.35 | 1.1.7 | - | 7 zuwa 9.5 | 2.75 zuwa 4 | - |
Farashin 690 | 0.05 | 0.5 | 0.5 | 0.015 | 0.03 | 27 zuwa 31 | ≥58 | 7 zuwa 11 | - | - | ≤0.5 | - | - | - |
Alloy dukiya m
Daraja | jihar | Ƙarfin ƙarfi RmN/m㎡ | Ƙarfin Haɓaka Rp0.2N/m㎡ | Tsawaita Kamar% | Brinell taurin HB |
Alloy20cb-3 | Magani Magani | 600 | 320 | 35 | - |
Alloy28 | Magani Magani | 680 | 347 | 37 | - |
Alloy31 | Magani Magani | 650 | 350 | 35 | 25 |
Alloy33 | Magani Magani | 770 | 320 | 34 | - |
Alloy75 | Magani Magani | 750 | 310 | 37 | - |