Haɗaɗɗen Zazzabi

◆ Haynes-188 yana da high high zafin jiki ƙarfi, mai kyau anti-oxidation da anti-lalata Properties, yadu amfani da aerospace, petrochemical, shipbuilding da sauran filayen.

Abubuwan sinadaran

Daraja

C

Si

Mn

S

P

Cr

Ni

Fe

B

Co

W

La

sauran

babu girma fiye

Haynes-188

0.05 zuwa 0.15

0.2 zuwa 0.5

1.25

0.015

0.02

21 zuwa 23

20 zuwa 24

≤3

≤0.015

40 zuwa 45

13 zuwa 15

0.03 zuwa 0.15

-